发明名称 Method and system for suppressing formation of scale defects during hot finish rolling
摘要 A plurality of finishing mills for finish rolling a rolled material are arranged in a row to construct a finishing mill group, 1st to 3rd surface coolers for cooling the surfaces of the rolled material are provided on the entrance side of the 1st to 3rd finishing mills of the fishing mill group, and the range of cooling of the rolled material by the surface coolers are set to be a range of 0.3 to 1.5 m toward the upstream side from a position separated by 1.5 m or less from the center of the work rolls of each of the finishing mills toward the entrance side of each of the finishing mills.
申请公布号 US6067836(A) 申请公布日期 2000.05.30
申请号 US19980201858 申请日期 1998.12.01
申请人 MITSUBISHI HEAVY INDUSTRIES, LTD. 发明人 KAYA, AKIRA;MIZUTA, KEIJI;FUKUMORI, JUNSOU;MIN, KYUNG-ZOON;LEE, JAE-YOUNG;SEO, YOUNG-GIL;PARK, JUNG-DO
分类号 B21B1/26;B21B45/02;B21B45/08;C21D9/52;C21D9/573;(IPC1-7):B21B27/06 主分类号 B21B1/26