发明名称 |
FE-CR ALLOY WITHOUT RIDGING |
摘要 |
PURPOSE: A Fe-Cr alloy is provided which exhibits a good ridging resistance and has an excellent formability and a percentage of elongation without annealing the high-temperature processed sheet before being cold reduced. CONSTITUTION: The Fe-Cr alloy comprises of 0.08 wt.% or less of C; about 8 wt% or more of Cr; 1.5 wt.% or less of Mn; less than 0.020 wt.% of Al; 0.05 wt.% or less of N; 1.5 wt.% or less of Si; less than 2.0 wt.% of Ni, 0.1 wt.% or more of Ti; and the balance being Fe and remaining elements; wherein the {multiply Ti(wt.%) by N(wt.%)}/Al(wt.%) is at least 0.14 and the Ti content satisfies the following equation: (Ti/48)/{(C/12)+(N/14)}>1.5.
|
申请公布号 |
KR20000022016(A) |
申请公布日期 |
2000.04.25 |
申请号 |
KR19980056359 |
申请日期 |
1998.12.18 |
申请人 |
ARMCO INC. |
发明人 |
YOSITTAKKE EIJO;MACKAGUE ALLAN R. |
分类号 |
C21D8/02;C22C38/18;C22C38/50;(IPC1-7):C22C38/18 |
主分类号 |
C21D8/02 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|