摘要 |
PROBLEM TO BE SOLVED: To obtain an intumescent mixture producible at <100 deg.C, not corroding a contacting part of a processing machinery with a product and a mold giving a form, and showing an improved expansion behavior. SOLUTION: This mixture for producing an intumescent molding product has a following composition: 30-60 wt.% thermoplastic resin, 40-70 wt.% intumescent graphite and 5-40 wt.% filler mixture. In the mixture for producing the intumescent molding product in which the total amount of components is 100 wt.%, the filler mixture comprises so as to form OH- ion in relation to the moisture content.
|