摘要 |
<p>A method of making activated carbon of various pore size distributions involves a providing oxidized pitch, carbonizing the pitch when the softening point of the pitch is less than about 250 °C, and activating the pitch to produce activated carbon. A catalyst metal can be included with the pitch to produce mesoporosity in the activated carbon.</p> |