发明名称
摘要 <p>A polyimide adhesive is applied in liquid form between surfaces of a pressure transducer glass surface and a glass pedestal tube and maintained at room temperature, or below, for a period of 10-15 hours to allow the adhesive solvent to evaporate. After such time, the temperature of the transducer and attached pedestal tube is elevated over a period of time to about 320 DEG C. to completely imidize the polyimide adhesive. The pedestal is then fixed within an opening in a base portion of a case, and electrical conductors are connected between pins in the case and transducer contacts. A cover is hermetically sealed to the case to thereby encase the transducer.</p>
申请公布号 JP2979233(B2) 申请公布日期 1999.11.15
申请号 JP19900018106 申请日期 1990.01.30
申请人 DORETSUSA NAGANO INC 发明人 UIRIAMU SUTEIIUN KOSHU
分类号 C03C27/10;A47G19/22;C09J135/00;C09J179/08;G01L9/00;(IPC1-7):C03C27/10 主分类号 C03C27/10
代理机构 代理人
主权项
地址