发明名称 Method of manufacturing a thin film magnetic recording medium having low MrT value and high coercivity
摘要 A method for manufacturing a magnetic disk includes the step of providing first and second magnetic layers on a substrate. The first magnetic layer comprises Co. The portion of the first magnetic layer comprising Cr, Ta, Ti, W, Zr or Hf, if any, is less than 7.5 atomic % of the first magnetic layer (and preferably less than 5 atomic %). The second magnetic layer also comprises Co, and more than 7.5 atomic % of the second layer is Cr, Ta, Ti, W, Zr or Hf (and preferably more than 10 atomic %). We have discovered that the first and second magnetic layers can be made very thin without having a great reduction in coercivity.
申请公布号 US5840394(A) 申请公布日期 1998.11.24
申请号 US19970829995 申请日期 1997.04.02
申请人 KOMAG, INCORPORATED 发明人 RANJAN, RAJIV YADAV;LU, MIAOGEN
分类号 G11B5/66;(IPC1-7):G11B5/66 主分类号 G11B5/66