摘要 |
Material selected from the group consisting essentially of molybdenum, arsenic, antimony, bismuth, copper, silver, potassium dichromate and iron chromite, is added during the manufacture of soda-lime-silica float glass to reduce the occurrences of nickel sulfide stone defects. Material is added in sufficient amounts such that the resulting glass is at least 0.010 wt. % of the selected material. In a preferred embodiment of the invention, molybdenum is added in the form of sodium molybdate such that the resulting glass is at least 0.015 wt. % molybdenum.
|