发明名称 DRY BARREL POLISHING INORGANIC MEDIA
摘要 PROBLEM TO BE SOLVED: To enable even rough finish polishing by dry barrel polishing by sintering a mixed material of argillaceous particulates, abrasive particles and aluminium hydroxide particulates as a small grain shape. SOLUTION: In dry barrel polishing inorganic media by sintering a mixed material of argillaceous particulates and abrasive particles as a binding material, aluminium hydroxide is added to and mixed in the mixed material. By the aluminium hydroxide, the media can be formed not only as a cutting quality maintenance preferential type and but also can be formed as a wear-tear restraint preferential type by adjusting its adding quantity, but when 5wt.% or more is contained, a shape of the media largely collapses by sintering, and since the media having a desired shape is hardly obtained, it is desirable that 5wt.% or less be contained for a general use.
申请公布号 JPH10146749(A) 申请公布日期 1998.06.02
申请号 JP19960304430 申请日期 1996.11.15
申请人 SINTO BRATOR CO LTD 发明人 IKEDA YASUSHI;ISHIDA TAKAO
分类号 B24B31/14;B24D3/04;C09K3/14;(IPC1-7):B24B31/14 主分类号 B24B31/14
代理机构 代理人
主权项
地址
您可能感兴趣的专利