Method of producing a split leather, especially for automotive applications subject to temperature and humidity fluctuations |
摘要 |
Between a chrome tanning step and a fat liquor treatment step, a flesh side split leather is subjected to shaving on both its split and flesh sides to a thickness of 1.1 to 2.5 mm, preferably 1.2 to 1.5 mm and is then aftertanned. After a split side dressing of the dried butt, a further shaving operation is effected on the flesh side to a thickness of 0.5 to 1.0 mm, preferably 0.7 to 0.9 mm, whereupon the flesh side is also dressed. The result is a split leather which is particularly effective for use on automotive vehicle dashboards and has low shrinkage even when subjected to high temperature and moisture fluctuations.
|
申请公布号 |
US5269814(A) |
申请公布日期 |
1993.12.14 |
申请号 |
US19900624221 |
申请日期 |
1990.12.04 |
申请人 |
LUDW. LINDGENS GMBH & CO. KG |
发明人 |
SCHMIDT, GUNTER;MEURER, PETER |
分类号 |
B05D7/24;C14B1/00;C14B1/02;C14B13/00;C14C3/06;C14C9/02;C14C11/00;(IPC1-7):C14C3/06;C14C3/28 |
主分类号 |
B05D7/24 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|