发明名称 |
THERMOPLASTIC RESIN MOLDING |
摘要 |
<p>PROBLEM TO BE SOLVED: To provide a rubber component-containing thermoplastic resin molding hardly causing deformation and crack. SOLUTION: This molding comprises a thermoplastic resin containing 5-40wt.% of a granular rubber component. The ratio b/a of an average major axis length (b) of a rubber particle 1 to an average minor axis length (a) of a rubber particle measured in a section within 30μm thickness from the surface of the molding at plural parts of the molding is <=2, the ratio of the maximum (b/a max) to the minimum (b/a min.) is in a range of 1<=(b/a max.)/(b/a min.)<=1.5 in a correlation of each section and the maximum Amax. and the minimum Amin. in correlation of the ratio of a rubber-occupied area at each section are in a range of 0<=(Amax.-A)/A<=0.2 and 0<=(A-Amin.)/A<=0.2 when the total ratio of the cross section area of the rubber particle 1 (rubber-occupied area ratio) is A%.</p> |
申请公布号 |
JPH09194599(A) |
申请公布日期 |
1997.07.29 |
申请号 |
JP19960005443 |
申请日期 |
1996.01.17 |
申请人 |
SUMITOMO CHEM CO LTD;SUMIKA A B S LATEX KK |
发明人 |
MATSUMOTO MASATO;KITAYAMA TAKEO;OGURA KIYOSHI;SHINOHATA MASAHIRO |
分类号 |
C08J5/00;C08F255/08;C08F279/00;C08J7/06;C08K5/00;C08K7/00;C08K7/16;C08L21/00;C08L25/12;C08L55/02;C08L101/00;(IPC1-7):C08J5/00 |
主分类号 |
C08J5/00 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|