发明名称
摘要 PURPOSE:To obtain a wire comprising heat resistance and flame resistance and flexibility, by coating the wire with the compound obtained by mixing a predetermined quantity of ethylene group copolymer resin and a predetermined quantity of chlorinated polyethylene having the predetermined characteristic. CONSTITUTION:The flame resistant agent at 5-50 weight part is mixed with the polymer at 100 weight part obtained by blending chlorinated polyethylene, which satisfies chlorine content at 15-28weight%, heat of dissolution of crystal at 2-14cal/g, melt flow rate at 1-12g/10min, in a range of 95-50 weight ratio and ethylene group copolymer resin in a range of 5-50 weight ratio. A wire comprising high heat resistance, high flame resistance and high flexibility can be obtained by coating on a bore wire the bridged insulating material of flame resistance and electrical insulating property, which material is obtained in this way.
申请公布号 JP2600935(B2) 申请公布日期 1997.04.16
申请号 JP19890330174 申请日期 1989.12.20
申请人 发明人
分类号 H01B3/44;H01B7/29 主分类号 H01B3/44
代理机构 代理人
主权项
地址