发明名称 FIBER HAVING HIGH SMOOTHNESS, FABRIC-LIKE MATERIAL AND MOLDING
摘要 PROBLEM TO BE SOLVED: To form a nonwoven fabric, a knitted or woven fabirc or a fiber forming body having good uniformity by using a highly smoothing fiber, obtained by applying a specific resin mixture composition to the surface of a thermoplastic fiber SOLUTION: An alkylphosphoric acid salt having a 6-14 average carbon number and/or a polyoxyalkylene adduct to an alkylphosphoric acid salt of a 10-22 average carbon number in an amount of 50-85wt.% is blended with 15-50wt.% of an amide group-containing polyoxyalkylene-modified silicone to prepare a smoothing agent. This, agent in an amount of 0.1-2.0wt.% is applied to a conjugate short fiber having <=30mm fiber length so as to arrange that at least a part of the fiber surface is formed by using a polyolefin-based resin, a polyester-based resin, a polyamide-based resin or on ethylene-acrylic ester- maleic anhydride terpolymer all having <=120 deg.C melting point as at least one component of the fiber and a thermoplastic resin having a melting point which is 20 deg.C higher than those of the above components is contained as the other component to provide the object fiber having high smoothness.
申请公布号 JPH0967772(A) 申请公布日期 1997.03.11
申请号 JP19950248774 申请日期 1995.08.31
申请人 CHISSO CORP 发明人 NISHIJIMA MASARU;SUZUKI MASAYASU
分类号 D01D5/30;D01F8/14;D04H1/549;D04H1/55;D04H3/011;D06M13/02;D06M13/244;D06M13/282;D06M13/292;D06M15/643;D06M15/647;D06M101/00;D06M101/16;D06M101/18;D06M101/30;D06M101/32;D06M101/34 主分类号 D01D5/30
代理机构 代理人
主权项
地址