PCT No. PCT/RU95/00222 Sec. 371 Date Apr. 9, 1998 Sec. 102(e) Date Apr. 9, 1998 PCT Filed Oct. 10, 1995 PCT Pub. No. WO96/17393 PCT Pub. Date Jun. 6, 1996A method for producing a battery electrode which includes the steps of: 1) mixing active material, methyl methacrylate/butadiene copolymer binder, and water; 2) drying the mixture so that it contains between 1% to 3.5% by weight of residual moisture; and 3) applying the dried material to a current collector. The novelty of this invention resides in drying the active material mixture prior to applying the mixture to the current collector. |