摘要 |
PROBLEM TO BE SOLVED: To save material and satisfy predetermined necessary conditions concerning stability, by making a reinforcing layer thin and by curing polymerizable, cool curable, and reactive(meta)acrylates prayed over the rear of the formation of acrylic glazing. SOLUTION: A) comprises 30-100 wt.% (meta)acrylate, 100 wt.% or less methyl(meta)acrylate or the like, 50 wt.% or less >=C5 (meta)acrylate or the like, and 30 wt.% or less atomatic vinyl substance or the like. B) comprises 5 parts or less (pre)polymer which can be dissolved or swollen in A) based on one part A), and C) comprises 7 parts or less plasticizer based on A)+10 parts B). It contains D) promoter and dolex system whose amounts are sufficient for cool curing the polymerization components of a system until they are polymerized, E) additive, F) 1-70 wt.% filler having 100 μm or smaller fineness that is inert tunder depolymerization conditions based on the total of A)-F), G) 10-50 wt.% glass fiber hexyl based on the total of A)-H), and H) 15 wt.% or less solvent based on the total of A)-E)+H). |