<p>PURPOSE: To effectively utilize a dephosphorized/desulfurized slag which have been difficult conventionally to use as a part of a cement starting material, etc., and have been disposed. CONSTITUTION: 2-5 pts.wt. dephosphorized/desulfurized slag regulated to <=1000ppm in a chlorine content incorporated in the slug and to <=15wt.% in a granular iron amount by controlling a cooling water for a molten slag generating at desulfurizing stage and dephosphorizing stage as a molten iron pretreatment and a magnetic separation/removal treating condition, is compounded with 140 pts.wt. cement clinker starting material and burned. In this way, the dephosphorized and desulfurized slag can be used as a part of the cement clinker starting material hardly causing influence on compression strength and coagulation of the cement.</p> |
申请公布号 |
JPH08198647(A) |
申请公布日期 |
1996.08.06 |
申请号 |
JP19950005832 |
申请日期 |
1995.01.18 |
申请人 |
NIPPON STEEL CORP;NIPPON STEEL CHEM CO LTD |
发明人 |
IGAWA JUNJI;MUTA MOTOHIRO;YOKOO MASAYOSHI;TANAKA SHIGEMORI;OYAMADA RYOICHI;SADATSUNE KAZUO;OGURA TOYOSHIGE |
分类号 |
C04B5/00;C04B7/02;C04B7/147;C04B7/38;(IPC1-7):C04B7/147 |
主分类号 |
C04B5/00 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|