发明名称 Using broken-up cupola furnace slag as additive
摘要 <p>Broken up cupola furnace slag is used to produce self-levelling floors by adding the slag in particle size 0-0.5mm and 60-80 wt. % to additives such as flowing agents and stabilisers and water and cement with a WZ factor of 0.4-0.7. The flowing agent, stabiliser, water and cement make up 20-40 wt. % of the mixture.</p>
申请公布号 DE19533999(C1) 申请公布日期 1996.05.15
申请号 DE1995133999 申请日期 1995.09.14
申请人 BILKE, THOMAS, 06526 SANGERHAUSEN, DE;BILKE, LUTZ, 06526 SANGERHAUSEN, DE 发明人 BILKE, THOMAS, 06526 SANGERHAUSEN, DE;BILKE, LUTZ, 06526 SANGERHAUSEN, DE
分类号 C04B18/14;E04F15/12;(IPC1-7):C04B18/14;E01C7/10 主分类号 C04B18/14