发明名称 |
METHOD FOR APPLYING POLYMER MODIFIED ASPHALT COATING TO CORRUGATED PIPES |
摘要 |
A method of coating a corrugated pipe (20) includes preparing an asphalt composition (30) having a polymer constituent within the range of from about 3 to about 20 percent, the composition (30) having a softening point within the range of from about 180.degree.F (82.degree.C) to about 250.degree.F (121.degree.C), and a viscosity at a temperature of 360.degree.F (182.degree.C) within the range of from about 600 (0.6 Pa s) to about 4000 cps (4 Pa s), heating the asphalt composition (30) to a temperature within the range of from about 340.degree.F (171.degree.C) to about 390.degree.F (199.degree.C), and coating the corrugated pipe (20) by positioning at least a portion of the corrugated pipe (20) in the heated asphalt composition (30) for a time sufficient for the corrugated pipe (20) to reach a temperature of at least 150.degree.F (66.degree.C). The coated pipe (20) is then removed from the asphalt composition (30) for cooling.
|
申请公布号 |
CA2155904(A1) |
申请公布日期 |
1996.03.01 |
申请号 |
CA19952155904 |
申请日期 |
1995.08.11 |
申请人 |
OWENS CORNING |
发明人 |
JANICKI, RICHARD T.;KEATING, JAY WALTER |
分类号 |
B05D1/18;F16L57/00;F16L58/10;(IPC1-7):B05D1/18 |
主分类号 |
B05D1/18 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|