发明名称 METHOD FOR CONTINOUS CASTING OF BORON ADDITION STEEL
摘要 The method, for casting boron-added steel which consists of (in wt.%) C of 0.003-0.10%, P of below 0.015%, S of below 0.015%, Sol.Al of 0.02-0.08%, N of 0.003-0.008%, B of 0.002%-0.010%, Mn, and balance Fe, has the characteristics that the Mn content is over 0.2%, the overheating degree of molten steel is over 35 deg.C, and the secondary cooling coefficient(K) is 0.1-0.2
申请公布号 KR950012630(B1) 申请公布日期 1995.10.19
申请号 KR19930031051 申请日期 1993.12.29
申请人 POSCO;RIST 发明人 IM, MUN - SOK;KIM, JIN - IL;YANG, SUNG - MAN;CHOE, JU
分类号 B22D11/00;(IPC1-7):B22D11/00 主分类号 B22D11/00