Alloy sheet for shadow mask and method for manufacturing thereof. |
摘要 |
An alloy sheet containing Fe, Ni and Cr has an average austenite grain size of 15 to 45 mu m and a degree of mixed grain for austenite grain size of 50% or less; said alloy sheet has a gathering degree of {331} plane on a surface of said alloy sheet being 35% or less, that of {210} plane 20% or less and that of {211} plane 20% or less; said degree of mixed grain is expressed by an eqution of (¦0.5 Dmax - D¦/D) x 100 (%), where D is an average austenite grain size, and Dmax is a maximum austenite grain size in said alloy sheet. A method for manufacturing an alloy sheet for a shadow mask comprising the steps of (a) hot-rolling, (b) annealing of hot-rolled sheet, (c) cold-rolling, (d) recrystallization annealing, (e) finish cold-rolling, (f) stress relief annealing and (g) annealing before press-forming. |
申请公布号 |
EP0641866(A1) |
申请公布日期 |
1995.03.08 |
申请号 |
EP19940102719 |
申请日期 |
1994.02.23 |
申请人 |
NKK CORPORATION |
发明人 |
INOUE, TADASHI, C/O INTELLECTUAL PROPERTY DEPT.;TSURU, KIYOSHI, C/O INTELLECTUAL PROPERTY DEPT.;YAMAUCHI, KATSUHISA, C/O INTELLECTUAL PTY DEPT.;HIASA, MICHIHITO, C/O INTELLECTUAL PROPERTY DEPT. |
分类号 |
C21D8/02;C21D9/46;C22C38/00;C22C38/54;H01J9/14;H01J29/07 |
主分类号 |
C21D8/02 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|