发明名称 Prepn. of propylene! copolymer for foaming sealable foils - by catalytic random copolymerisation to high reduced specific viscosity and degradation by melt extrusion
摘要 A C3H6 copolymer, (I), is produced in 2 steps, by (I) preparing a random copolymer having reduced specific viscosity, RSV, 4-8 dl./g., by copolymerising a mixt. contg. by wt., either (a) 94-5-99.5% C3H6 with 0.5-6.5% C2H4 or (b) 85-97.5% C3H6, 0.5-5% C2H4 and 2-10%, w.r.t. total mixt., of another l-olefin having formula CH2=CHR (where R is 2-6C alkyl) in the presence of H2 as mol. wt. regulator, a catalyst and opt. a dispersant, and (2) degrading the copolymer by melt extrusion at 200-300 degrees C. in the absence of O2 and radical-donors, to reduce mol. wt. to RSV 1.8-3.5 dl./g. The catalyst in (1) consists of a Ti-contg. solid component, an organic Al component and opt. 1 or more cpds. having electron-donor character. (I) forms foils which retain their sealability also after preliminary printing. By controlling RSV in step (1), soluble polymer quantity is no higher than that obtd. by C3H6 homoplymerisation. The suspension is easily pumped and polymer powder is easily separated.
申请公布号 FR2429231(A1) 申请公布日期 1980.01.18
申请号 FR19790016235 申请日期 1979.06.25
申请人 HOECHST AG 发明人
分类号 C08F8/50;C08F210/06 主分类号 C08F8/50
代理机构 代理人
主权项
地址