发明名称 |
Quantification of blast furnace slag in a slurry |
摘要 |
A method is provided to determine the concentration of an amorphous material such as blast furnace slag in a slurry such as drilling fluid, completion fluid fluids. A sample is annealed at a temperature between about 800 degrees C. and about 1000 degrees C. for a time period of about six hours to form crystals from the amorphous material, and the sample along with a known amount of a standard is then analyzed by X-ray diffraction. This method is particularly useful in determining the amount of blast furnace slag in a drilling fluid prior to conversion of the drilling fluid to a wellbore cement slurry by addition of additional blast furnace slag.
|
申请公布号 |
US5285679(A) |
申请公布日期 |
1994.02.15 |
申请号 |
US19920964981 |
申请日期 |
1992.10.22 |
申请人 |
SHELL OIL COMPANY |
发明人 |
JACKSON, WILLIAM E.;MURRAY, THOMAS E.;HALE, ARTHUR H. |
分类号 |
G01N1/44;G01N5/04;G01N23/20;G01N33/24;(IPC1-7):G01N5/04 |
主分类号 |
G01N1/44 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|