摘要 |
A method of improving strength in aluminum alloys. The method involves solution heat treating an aluminum alloy product, quenching the alloy product, warm working the alloy product without a pre-aging step, and aging the alloy product at 250 DEG -400 DEG F. (121 DEG -204 DEG C.). The method may be used on forgings, to impart T8-type hardness to alloys that previously could only obtain such hardness levels in non-forging applications, such as by using stretch/cold working techniques.
|