发明名称 STEELMAKING METHOD USING COPPER AND TIN-INCORPORATING SCRAP AS RAW MATERIAL
摘要 <p>PURPOSE:To obtain a molten steel having <0.1wt.% content of copper or tin by using iron scrap incorporating much copper or tin. CONSTITUTION:The iron scrap 3 is charged into a converter 1 and heated at >=1000 deg.C, and at the time of melting about 10wt.% of the scrap, the obtd. molten material is discharged to the outside of the furnace and successively, the residual iron scrap is melted, and if necessary, the other scrap or molten iron from a blast furnace incorporating no copper and tin is further charged to execute steelmaking.</p>
申请公布号 JPH04297518(A) 申请公布日期 1992.10.21
申请号 JP19910060482 申请日期 1991.03.25
申请人 SUMITOMO METAL IND LTD 发明人 HIRATA TAKEYUKI
分类号 C21C5/28;C21C5/52 主分类号 C21C5/28