发明名称 PRODUCTION OF CARBONATE-CONTAINING HYDROXYAPATITE WHISKER
摘要 PURPOSE:To easily obtain the title whiskers having a large average length in a short time by heating an aq. soln. contg. calcium salt, phosphoric acid and/or phosphate and urea at a prescribed temp. and heating the resulting liq. reaction product under prescribed conditions. CONSTITUTION:An aq. sol. contg. calcium salt and phosphoric acid and/or phosphate is heated at 70-90 deg.C in the presence of urea to form octacalcium phosphate whiskers having >=100mum average length. The resulting liq. reaction product contg. the whiskers is then heated at 90-180 deg.C. Carbonate-contg. hydroxyapatite whiskers having >=50 mum average length are formed.
申请公布号 JPH0416600(A) 申请公布日期 1992.01.21
申请号 JP19900120558 申请日期 1990.05.09
申请人 KARUSHIIDO:KK 发明人 KINOSHITA MAKIO;KISHIOKA AKIRA;ITAYA SEIJI;MATSUDA KENICHIRO;SEGAWA KAZUHIRO;SASAKI NAOHIKO;MITO HITOSHI
分类号 A61L24/00;A61K6/033;A61L27/00;C30B29/62 主分类号 A61L24/00
代理机构 代理人
主权项
地址