发明名称 |
CUSHION MATERIAL AND METHOD FOR PREPARATION THEREOF |
摘要 |
The cushion material according to the invention is prepared by mixing (A) polyester fibers having a fineness of 4 to 30 denier and a cut length of 25 to 150 mm with (B) core-sheath type conjugated fibers having a fineness of 2 to 20 denier and a cut length of 25 to 76 mm in a weight ratio of 95 SIMILAR 40 : 5 SIMILAR 60, the sheath component of said conjugated fibers having a melting point lower than that of the core component of said conjugated fibers and said polyester fibers with a difference of 30 DEG C or more. In the cushion material, cubically and continuously interconnected portions of the fibers are adhered by fusion of the sheath portion of the above core-sheath type conjugated fibers. The cushion material having a thickness of 10cm or more and a good quality can be stably prepared by combining far-infrared ray or hot air flow heating and steaming in the heat-treatment. |
申请公布号 |
EP0371807(A3) |
申请公布日期 |
1990.09.19 |
申请号 |
EP19890312490 |
申请日期 |
1989.11.30 |
申请人 |
KANEBO LTD. |
发明人 |
NOHARA, SABURO;MASUDA, YUGORO |
分类号 |
B68G1/00;D04H1/435;D04H1/541 |
主分类号 |
B68G1/00 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|