摘要 |
The present invention is a polymeric composition with improved extrudability comprising a vinylidene chloride interpolymer and a Group IIA alkaline-earth hydroxyphosphate, which is incorporated with the vinylidene chloride interpolymer by advance addition, polymer slurry addition or, finally, by dry blending addition. The Group IIA alkaline-earth hydroxyphosphate will be present in an amount of between about 0.01 to about 5 weight percent, said weight percents being based on the total weight of the polymeric composition.
|