发明名称 STEEL WIRE FOR MAG WELDING
摘要 PURPOSE:To reduce a spatter and to improve the shape of a bead by containing C, Si, Mn, S, Ti, O in a specific wt.%, and balance Fe and limiting the value of CXO and the mixture amt. of Al and N at <=a specific %. CONSTITUTION:The composition of a wire is taken as 0.005-0.04% (weight is same on the rest) C, 0.30-0.80% Si, 1.40-2.40% Mn, 0.01-0.035% S, 0.05-0.15% Ti, 0.0030-0.025% C, the Al to be mixed is regulated <=0.020% and N <=0.0050%, the value of CXO is limited to <=4X10<-4> and the balance is taken as Fe and impurities. The C, S components refines the spatter droplet and the generation of CO gas can be restrained with the limitation of the CXO value, so the large granulation of spatters is prevented and the generation amt. is reduced as well. The bead shape is improved because of the S component preventing the generation of a bead undercut.
申请公布号 JPS63157794(A) 申请公布日期 1988.06.30
申请号 JP19860305808 申请日期 1986.12.22
申请人 NIPPON STEEL CORP 发明人 YAMASHITA KOZO;KOYAMA HIROSHI;TANAKA TAKAYOSHI
分类号 B23K35/30 主分类号 B23K35/30
代理机构 代理人
主权项
地址