A matrix (16) for holding the electrolyte within a phosphoric acid fuel (12) is made from silicon carbide and a binder of polyethersulfone. Preferably the matrix consists of 10-20 weight percent polyethersulfone with a balance of silicon carbide. The matrix has improved strength, wettability and bubble pressure compared to the best known prior art matrix.
申请公布号
DE3470820(D1)
申请公布日期
1988.06.01
申请号
DE19843470820
申请日期
1984.07.18
申请人
UNITED TECHNOLOGIES CORPORATION
发明人
TROCCIOLA, JOHN, CHARLES;POWERS, JOSEPH;MARTIN, RONALD, GEORGE