<p>Inorganic resins are formed by mixing: (a) a liquid component A comprising an aqueous solution of one or both of mono aluminum phosphate and mono magnesium phosphate, the solution having a viscosity of from 700 to 10,000 centipoises; and (b) a liquid component B comprising an aqueous vehicle, a phosphate-reactive constituent which is one or both of wollastonite and magnesium oxide, and a non-reactive dispersing agent, component B having a viscosity permitting it to be rapidly and thoroughly mixed with component A so as to form a slurry which reacts exothermically to form an inorganic resin. Such inorganic resins may be obtained in non-cellular or cellular form.</p> |