摘要 |
<p>PCT No. PCT/JP83/00210 Sec. 371 Date Mar. 1, 1984 Sec. 102(e) Date Mar. 1, 1984 PCT Filed Jul. 1, 1983 PCT Pub. No. WO84/00240 PCT Pub. Date Jan. 19, 1984.A magnetic recording medium has, on a nonmagnetic support, a magnetic layer consisting mainly of an acicular iron oxide magnetic powder and a binder. In order to improve the S/N ratio, a fine magnetic powder having a specific surface area as determined by the BET method, of not less than 35 m2/g is used. In order to improve the dispersibility of the magnetic powder and to improve the squareness ratio and durability thereof, the binder contains a resin which has a molecular weight of not more than 50,000 and has at least one polar group selected from the group consisting of polar groups having the general formulas: <IMAGE> (wherein M is hydrogen, lithium, sodium or potassium; and M1 and M2 are hydrogen, lithium, sodium, potassium or alkyl groups.</p> |