发明名称 PRODUCTION OF COLD ROLLED AUSTENITIC STAINLESS STEEL STRIP HAVING LESS SURFACE DEFECTS
摘要 PURPOSE:To considerably decrease the generation of micro-surface defects by adding an atm. annealing stage and pickling state between a grinding stage and cold rolling stage in a process for producing a cold rolled steel strip of an austenitic stainless steel. CONSTITUTION:The steel strip hot rolled from a slab is subjected to annealing and pickling - grinding - cold rolling - annealing and pickling - temper rolling in the method for producing the cold rolled austentic stainless steel strip. The atm. annealing stage and pickling stage are added between the grinding stage and the cold rolling stage among these stages. The steel strip hardened to about 245 Vickers hardness by grinding with the grinder is annealed in the atm. to <=200 Vickers hardness and after the oxide scale formed during such annealing is pickled away, the strip is treated by the stages after the cold rolling. The micro-defects on the surface of the austenitic stainless steel sheet as the final product are considerably decreased.
申请公布号 JPS61266587(A) 申请公布日期 1986.11.26
申请号 JP19850109677 申请日期 1985.05.22
申请人 KAWASAKI STEEL CORP 发明人 SHIOKAWA TAKASHI;TAKEDA MOTOHIKO;MURABAYASHI MINORU;ISHIKAWA MASAAKI
分类号 B21B1/22;B21B3/02;C21D9/52;C23F17/00;C23G3/02 主分类号 B21B1/22
代理机构 代理人
主权项
地址
您可能感兴趣的专利