摘要 |
A synthetic vascular graft of internal diameter in the range of 0.1 mm to 20 mm and wall thickness between 0.075 mm and 2.0 mm is preferably made by electrostatic spinning of polymeric material. Under an elongation of between 5% and 25% over its unstressed state, the change in internal pressure from a first pressure to a second pressure, the difference between the first and second pressures lying in the range between 20 mm Hg and 75 mm Hg, undergoes a change in internal diameter substantially equal to the change in internal diameter experienced when a corresponding natural artery stretched to an extend experienced in vivo is subjected to the same change in internal pressure. The graft is made by electrostatically spinning an organic polymer material. |