发明名称 METHOD FOR CONTINUOUSLY ANNEALING COLD ROLLED DEAD SOFT STEEL SHEET
摘要 PURPOSE:To manufacture a cold rolled steel sheet for deep drawing causing no secondary working crack by carrying out heating and cooling under specified conditions when a cold rolled dead soft steel sheet is continuously annealed. CONSTITUTION:A dead soft steel sheet is cold rolled and heated to a temp. above the recrystallization temp. to carry out continuous annealing. At this time, the cold rolled steel sheet is heated at >=1 deg.C/sec heating rate, and cooling is started within 5sec after finishing the heating. Thus, the fear that P is segregated is reduced, and secondary working crack is prevented.
申请公布号 JPS60106919(A) 申请公布日期 1985.06.12
申请号 JP19830214792 申请日期 1983.11.15
申请人 KAWASAKI SEITETSU KK 发明人 OBARA TAKASHI;SATOU SUSUMU;NISHIDA MINORU
分类号 C21D9/46;C21D9/48;C21D9/50;C21D9/56;(IPC1-7):C21D9/48 主分类号 C21D9/46