摘要 PURPOSE:The product ratio is reduced under 0.65 between external magnetic field intensity HDC, element saturation magnetization 4piMs and adverse magnetic field coefficient N of HDC direction. Furthermore, HDC is varied by negative temperature coefficient against temperature. Thus, the temperature characteristics can be improved.
申请公布号 JPS6019162(B2) 申请公布日期 1985.05.15
申请号 JP19750141322 申请日期 1975.11.26
申请人 FUJITSU LTD 发明人 TOKUMITSU YASUYUKI;SUMI HIROAKI;KASAHARA SHUNICHI;KANOCHI JUNICHI
分类号 H01P1/36;H01P1/32;H01P1/38;H01P1/383;H01P1/387;H01P1/39 主分类号 H01P1/36