发明名称 SULPHURIC ACID LEACHING OF LATERITIC NICKEL ORES
摘要 <p>Sulphuric acid leaching has been used in the treatment of lateritic ores for the recovery of nickel and cobalt therefrom. However, in order to obtain good extraction from these ores, prolonged treatment using acid of high strength and also using high pressures and recycling steps have been necessary. In the improved method of the invention nickel and cobalt is solubilized from high-magnesia nickeliferous serpentine ores by leaching the ore with an aqueous solution of sulphuric acid while adding to the solution a reducing agent to maintain the redox potential of the solution at a value between 200 and 400 millivolts, measured against the saturated calomel electrode. This improved procedure increases the reactivity of the serpentine and results in maximum extraction of nickel consistent with minimum extraction of iron and magnesia and minimum acid consumption.</p>
申请公布号 NZ198818(A) 申请公布日期 1984.07.06
申请号 NZ19810198818 申请日期 1981.10.30
申请人 FALCONBRIDGE NICKEL MINES LTD. 发明人 HATCH, W.R.;DUNN, R.R.
分类号 B01D11/00;B01F1/00;C01G53/10;C22B;C22B3/00;C22B23/00;(IPC1-7):22B3/00;22B23/04 主分类号 B01D11/00
代理机构 代理人
主权项
地址