发明名称 OZONE DECOMPOSING CATALYST
摘要 <p>PURPOSE:To obtain an ozone decomposing efficiency and excellent durability, by compounding Co-oxide, ni-oxide and Mn-oxide in a specific containing ratio. CONSTITUTION:This catalyst comprises three components, that is, Co-oxide (CoOx), NO and MnO2 and, with respect to the contents of the aforementioned components, CoOx is adjusted to 48-80mol%, NiO to 10-38mol% and MnO2 to 2-22mol%. As the result, an ozone decomposing catalyst having both high ozone decomposing efficiency and excellent durability not achieved by a CoRx catalyst or a CoOx-NiO catalyst is obtained. This catalyst can be prepared by a kneading method, a suspension precipitation method or the like. In addition, the shape of the catalyst may be a fine powder, a granule or a pellet having an arbitrary particle size, one obtained by coating the surface of a monolithic ceramic carrier with a catalyst or other shapes.</p>
申请公布号 JPS5966347(A) 申请公布日期 1984.04.14
申请号 JP19820176592 申请日期 1982.10.07
申请人 FUJI DENKI SOUGOU KENKYUSHO:KK 发明人 OCHIWA SHINICHI;HIROSE YOSHIKAZU;KUNIHARA KENJI
分类号 B01D53/86;B01J23/84;B01J23/889 主分类号 B01D53/86
代理机构 代理人
主权项
地址