发明名称 Lightweight material of glass fibre, gypsum and borax
摘要 Lightweight material is produced by mixing glass fibre with around 5% borax, adding gypsum in amt. 25-45%, followed by water in amt. 30-50%. The mixt. is then agitated for 2-12 mins. at 10-25 deg.C. - It is partic. useful for construction of false ceilings, slabs and tiles.
申请公布号 ES8402045(A1) 申请公布日期 1984.04.01
申请号 ES19550005238 申请日期 1983.07.05