摘要 A dramatic reduction in the time required to fine-grind high borate solder glasses is achieved. In the prior art method, the glass is ball-milled in the presence of an amine for about seven days or more. It has now been discovered that by first rod-milling such glasses for a period of from about 1/2 to about 24 hours, the time required for the "amine grind" can be shortened to a period of from about 1 to 3 days. A further improvement is that rod milling eliminates the laborious sieving procedure previously employed to ensure the absence of undesirably large particles in the feed to the amine grinding operation.