发明名称 Method of electrolytically recovering zinc
摘要 A lead alloy anode for a cell for the electrowinning or electrolytic recovery of zinc consists of 0.05 to 0.25% by weight strontium and/or 0.05 to 0.1% by calcium in combination with 0.1 to 0.5 silver, balance lead. The cell is used in a method for the recovery of zinc at, for example, a current density of 160 to 630 amp/m2, a temperature of 30 DEG to 46 DEG C. and an electrolyte containing 40 to 70 g/l zinc and 165 to 220 g/l sulfuric acid.
申请公布号 US4364807(A) 申请公布日期 1982.12.21
申请号 US19810233491 申请日期 1981.02.11
申请人 RUHR ZINK GMBH 发明人 VON ROEPENACK, ADOLF;STOCK, GUENTER;HEUBNER, ULRICH
分类号 C22C11/00;C22C11/02;C25C1/16;C25C7/02;C25D17/10;(IPC1-7):C25B11/03 主分类号 C22C11/00