摘要 |
<P>POUR AJUSTER LA COMPOSITION D'UN ALLIAGE POUR LA GALVANISATION AU TREMPE D'ACIERS, Y COMPRIS ACIERS AU SILICIUM, AVEC UNE COMPOSITION COMPRENANT DES TENEURS PONDERALES EXPRIMEES EN P.P.M., PLOMB 1000 A 15000, ALUMINIUM 100 A 5000, ETAIN 300 A 20000, MAGNESIUM 10 A 1000, ON AJOUTE A L'ALLIAGE, DEFICITAIRE EN AU MOINS UN ADDITIF, DES COMPOSITIONS METALLIQUES SOLUBLES DANS LE ZINC EN FUSION ET COMPORTANT UN ADDITIF A TENEUR RELATIVEMENT ELEVEE EN SUFFISANCE POUR COMPENSER LE DEFICIT; LA COMPOSITION D'ETAIN EST DE L'ETAIN PRATIQUEMENT PUR, LA COMPOSITION DE MAGNESIUM UN TERNAIRE ZINC, MAGNESIUM (5000 A 50000 P.P.M.) ET ALUMINIUM (10 A 500 P.P.M.), ET LA COMPOSITION D'ALUMINIUM EST UN BINAIRE ZINC ALUMINIUM CONTENANT ENVIRON 5 D'ALUMINIUM.</P>
|