An improved high temperature fatigue resistant coating for nickel and cobalt base superalloys having good oxidation and sulfidation resistance. The coating comprises by weight, 8-30% Co, 8-30% Cr, 5-20% Al, 10-60% Ni and 0.05-1.0% of a reactive metal selected from the group of Y, Sc, La and mixtures thereof, balance selected from the group consisting of Pt, Rh, and mixtures thereof, the (Pt+Rh) content being at least 13%.
|