摘要 |
<p>A process for the manufacture of a decorative laminate utilises a decorative laminate surface of overlay paper carrying a coating comprising a pigment and a binder. This coating affords improved printability without unacceptably reducing absorbency towards impregnating resins. The Gurley porosity of the coated paper is about 10-70 sec/100 ml; and the coating is present at a dry coatweight of up to 10gm-2, preferably 2.5 to 3gm-2. The coating is preferably applied by means of a size press. Laminate manufacture using the paper is conventional.</p> |