发明名称 SOLID DESICCATING AGENT
摘要 PURPOSE:To obtain a solid desiccating agent excellent in a moisture absorbing rate, a moisture absorbing capacity, long lasting property of moisture absorption or the like by a method wherein calcium chloride is mixed in zeolite and the resultant mixture is molded and solidified under pressure and, thereafter, the resultant molded mixture is baked by heating. CONSTITUTION:Zeolite and calcium chloride are mixed so as to adjust a ratio of calcium chloride to 10% or less in the wt. percent basis. Then, the resultant mixture is molded and solidified under pressure and, thereafter, the obtained molded object is heated and baked at 200-400 deg.C. The obtained solid desiccating agent prepared as described above has high moisture absorbing capacity even under a high humidity condition and excellent long lasting property as well as phenomena such as swelling due to water absorption, deliquescence, pulverization or the like can be controlled.
申请公布号 JPS5778944(A) 申请公布日期 1982.05.17
申请号 JP19800154633 申请日期 1980.11.05
申请人 TOUSHIYOKU:KK;ASADA SEIFUN KK 发明人 MORITA SHIGERU;YAMADA OSAMU
分类号 B01D53/28;B01J20/04;B01J20/16 主分类号 B01D53/28
代理机构 代理人
主权项
地址