发明名称 ANNEALING METHOD FOR COLD ROLLED STEEL PLATE
摘要 PURPOSE:To increase lubricity at the rolling and to reduce carbon stains after annealing by coating a specific coating agent on a cold-rolled steel plate by using rolling oil contg. no rust preventives prior to annealing said rolled steel plate. CONSTITUTION:Rolling oil contg. no rust preventives is coated on the surfaces of a steel plate and rolls and the steel plate is cold-rolled. Next, >=1 kinds of alcohols of 12-20 carbon numbers, monoesters of 18-28 carbon numbers, hydrocarbon polymers of 400-10,000mol.wts., and mineral oils of 8-120cst viscosisties (100 deg.F) are coated on the surfaces of this rolled steel plate. Thence, the steel plate coated with this coating agent is annealed.
申请公布号 JPS5735619(A) 申请公布日期 1982.02.26
申请号 JP19800109543 申请日期 1980.08.08
申请人 SUMITOMO METAL IND 发明人 MASE TOSHIAKI;YAMAMOTO HIDEO
分类号 B21B1/28;B21B45/00;B21B45/02;C21D1/26;C21D1/70;C21D1/72;C21D9/46 主分类号 B21B1/28
代理机构 代理人
主权项
地址