发明名称 REGENERATION METHOD OF ACTIVE CARBON CARRYING PHOSPHORUS COMPOUND
摘要 <p>PURPOSE:To improve the malodorous gas adsorption capacity of regenerated active carbon of lowered adsorption capacity carrying the oxide of phosphorus, the oxygen acid of phosphorus or its salt by heating the same to 350-700 deg.C which are above the decomposition temp. of phosphorus compounds. CONSTITUTION:The active carbon carrying at least one kind of the oxide of phosphorus, the oxygen acid of phosphorus or its salt and having been degraded of adsorption capacity by being contacted with basic malodorous component gases such as ammonia and amines is heated at 350-700 deg.C, whereby it is regenerated. The active carbon prepd. by using charcoal, coke, coconut shells, resins, etc. as raw materials, and generating the same and having 200-2,000m<2>/g specific surface areas may be used, and the amount of carrying the phosphorus compound in the active carbon is >=1/100 with respect to the active carbon. The proper regeneration of the active carbon of degraded malodorous gas adsorption performance is to heat the active carbon at 370-500 deg.C in the presence of an inert gas such as nitrogen or carbon dioxide.</p>
申请公布号 JPS5695334(A) 申请公布日期 1981.08.01
申请号 JP19790173820 申请日期 1979.12.28
申请人 TAKEDA CHEMICAL INDUSTRIES LTD 发明人 NISHINO HIROSHI;AIBE NORIO;TSUTSUMI YOSHIO
分类号 B01D53/38;B01D53/34;B01D53/81;B01J20/34;C01B31/08 主分类号 B01D53/38
代理机构 代理人
主权项
地址