VERFAHREN ZUR HERSTELLUNG VON CHROMARTIGEN LEGIERUNGEN |
摘要 |
<p>Iron-chromium alloys, such as stainless steels, are made in a direct arc DC electric arc furnace with a bath of molten steel scrap in the hearth and functioning as the anode with the arcing electrode cathodic, while feeding chromium-oxide to the bath at the arc spot on the bath's surface under conditions causing reduction of the oxide and addition of chromium to the bath.</p> |
申请公布号 |
DE2823234(A1) |