发明名称 PROCEDE D'OBTENTION D'UN CATALYSEUR A BASE DE CUIVRE NICKEL ET MANGABESE POUR LA REDUCTION DES COMPOSANTS TOXIQUES DES GAZ D'ECHAPPEMENT DES MOTEURS A COMBUSTION INTERNE
摘要 1465986 Exhaust gas purification catalysts HOECHST AG 12 Nov 1974 [24 Nov 1973] 48885/74 Heading BIE [Also in Division Cl] Catalysts comprise a ceramic honeycomb structure coated with a layer of alumina carrying copper, nickel and manganese oxides applied by impregnation after the coating of the carrier. They may be made by heating the honeycomb to 300-400‹C, introducing it while hot into a concentrated solution of an aluminium salt of a volatile acid for 15-60 min, blowing out excess solution, drying the carrier at room temperature, heating the dry carrier for 1-4 hr. at 350-450‹C, calcining at 500-700‹C for 2-6 hr., heating to 300-400‹C, dipping while hot into a hot concentrated solution of copper, nickel and manganese salts of volatile acids for 15-60 min, blowing out the excess solution, drying for 1-4 hr at 350-450‹C and calcining at 700-1000‹C for 5-20 hrs. The catalyst may be reduced by heating in an atmosphere containing a minor proportion of a gaseous reducing agent.
申请公布号 RO63718(A) 申请公布日期 1978.10.15
申请号 RO19740080585 申请日期 1974.11.23
申请人 HOECHST AG,DE 发明人 STENZEL,JUERGEN,DE
分类号 B01D53/94;B01J23/84;B01J23/889;B01J23/89;B01J35/04;B01J37/02;(IPC1-7):01J37/08 主分类号 B01D53/94
代理机构 代理人
主权项
地址