摘要 |
The present invention relates to methods for manufacturing paper or paperboard with improved strength, the methods comprising the addition of the reaction product of a cationic polyacrylamide and an aqueous aldehyde generating compound or a glyoxal releasing compound, or glyoxal itself, prepared at the mill site at high concentrations, then diluted and added into a fiber furnish prior to forming or drying of the paper or paperboard sheet.
|