发明名称 Verfahren zum tiegelfreien Zonenschmelzen
摘要 1,175,449. Floating zone-melting. SIEMENS A.G, 12 June, 1967 [15 June, 1966], No. 27106/67. Heading B1S. In the floating zone-melting of a silicon rod attached to a seed using an induction coil, the coil is eccentrically disposed with respect to the supply rod and the recrystallized rod for at least part of the operation. The coil may be reciprocated by rectilinear or circular movement of its axis at e.g. 9 alternations per minute between maximum and minimum eccentricity. The speed of passage of the molten zone may be 2 mm/min. The recrystallized rod may be rotated at 20 rpm. The cross-sectional area of the seed may be up to one tenth that of the supply rod. In steady operation, the diameter of both the supply and recrystallized rods may be larger than that of the coil. The supply and recrystallized rods may be on the same axis (Fig. 2) or may be offset (Fig. 5).
申请公布号 DE1519894(A1) 申请公布日期 1971.01.21
申请号 DE19661519894 申请日期 1966.06.15
申请人 SIEMENS AG 发明人 WOLFGANG KELLER,DR.;KONRAD REUSCHEL,DIPL.-CHEM.DR.
分类号 C30B13/28 主分类号 C30B13/28
代理机构 代理人
主权项
地址