摘要 A glass ceramic containing lithium-ions and having a garnet-like main crystal phase having an amorphous proportion of at least 5% is disclosed. The garnet-like main crystal phase preferably has the chemical formula Li7+x+yMxIIM3−xIIIM2-yIVMyVO12, wherein MII is a bivalent cation, MIII is a trivalent cation, MIV is a tetravalent cation, MV is a pentavalent cation. The glass ceramic is prepared by a melting technology preferably within a Skull crucible and has an ion conductivity of at least 5·10−5 S/cm, preferably of at least 1·10−4 S/cm.
申请公布号 US2016329598(A1) 申请公布日期 2016.11.10
申请号 US201615215421 申请日期 2016.07.20
申请人 SCHOTT AG 发明人 SCHNEIDER Meike;HOCHREIN Oliver;SCHMIDBAUER Wolfgang;KUNZE Miriam
分类号 H01M10/0562;H01M10/0525;C03C4/18;C03C21/00;C03C10/00;C03C3/12 主分类号 H01M10/0562
代理机构 代理人
主权项 1. A lithium-ion conducting glass ceramic comprising a garnet-like main crystal phase having an amorphous proportion of at least 5% wt.-%, wherein said garnet-like main crystal phase has the chemical formula: Li7+x-yMxIIM3−xIIIM2-yIVMyVO12,wherein MII is a bivalent cation, MIII a trivalent cation, MIV a tetravalent cation, MV a pentavalent cation.
地址 Mainz DE